Now showing items 1-11 of 11
Abstract: | Blends of polychloroprene rubber and plasticized polyvinylchloride have been prepared in various compositions and their properties evaluated. The properties of the blends show that they can be used to replace polychloroprene in many applications |
URI: | http://dyuthi.cusat.ac.in/purl/826 |
Files | Size |
---|---|
K E George and others,Blends of...,Dec1986.PDF | (4.998Mb) |
Abstract: | Ultra fine nickel ferrite have been synthesized by the sol-gel method. By heat treating different portions of the prepared powder separately at different temperatures, nano-sized particles of nickel ferrite with varying particle sizes were obtained. These powders were characterised by the X-ray diffraction and then incorporated in the nitrile rubber matrix according to a specific recipe for various loadings. The cure characteristics and the mechanical properties of these rubber ferrite composites (RFCs) were evaluated. The effect of loading and the grain size of the filler on the cure characteristics and tensile properties were also evaluated. It is found that the grain size and porosity of the filler plays a vital role in determining the mechanical properties of the RFCs |
Description: | Journal ofAppliedPolymer Science,Vol. 119, 3019–3025 (2011) |
URI: | http://dyuthi.cusat.ac.in/purl/4424 |
Files | Size |
---|---|
Cure Characteri ... n Nano-Nickel Ferrites.pdf | (692.2Kb) |
Abstract: | Fine particles of barium ferrite (BaFe12O19) were synthesized by the conventional ceramic technique. These materials were then characterized by the X-ray diffraction method and incorporated in the natural rubber matrix according to a specific receipe for various loadings of ferrite. The rubber ferrite composites (RFC) thus obtained have several applications, and have the advantage of molding into complex shapes. For applications such as microwave absorbers, these composites should have an appropriate dielectric strength with the required mechanical and magnetic properties. The N330 (HAF) carbon black has been added to these RFCs for various loadings to modify the dielectric and mechanical properties. In this article we report the effect of carbon black on the mechanical and dielectric properties of these RFCs. Both the mechanical and dielectric properties can be enhanced by the addition of an appropriate amount of carbon black |
Description: | Journal of Applied Polymer Science, Vol. 89, 769–778 (2003) |
URI: | http://dyuthi.cusat.ac.in/purl/4371 |
Files | Size |
---|---|
Effect of Carbo ... ntainingBarium Ferrite.pdf | (197.6Kb) |
Abstract: | The latex industry has expanded over the years to meet the world demands for gloves, condoms, latex thread etc. Because of the strict specifications for the products and the unstable nature of the latex, as high as 15%, of the final latex products are rejected. Since waste latex rubber (WLR) represents a source of high quality rubber hydrocarbon, it is a potential candidate for generating reclaimed rubber of superior quality. Two types of WLR with different amounts of polysulfidic bridges are used in these experiments, which are reclaimed with variation of the concentration of the reclaiming agents, the reclamation temperature and time, Di phenyldisultide, 2-aminophenyldisulfide and 2,2'-dibenzamidodiphenyldisulfide (DBADPDS) are used as reclaiming agents, and the effect of diphenyldisulfides (DPDS) with different substituents, on the reclamation efficiency of WLR is investigated. A kinetic study of the reclamation reaction with the three reclaiming agents is done. The reaction rates and activation energies are calculated and compared with literature values. The comparative study of the three different reclaiming agents shows that (DBADPDS) is able to break the crosslinks at temperature levels 20'C below the temperature levels normally used with DPDS. Another advantage of this reclaiming agent is the reduced smell during the reclamation process and of the final reclaims, one of the most important shortcomings of other disulfides used for this purpose. |
URI: | http://dyuthi.cusat.ac.in/purl/822 |
Files | Size |
---|---|
V V Rajan,Effec ... isulfides....Sept.2006.PDF | (12.78Mb) |
Abstract: | Prevulcanized natural rubber latex was prepared by the heating of the latex compound at 55°C for different periods of time (2, 4, 6, 8, and 10 h). The changes in the colloidal stability and physical properties were evaluated during the course of prevulcanization. The prevulcanized latex compounds were stored for 300 days, and the properties were monitored at different storage intervals (0, 20, 40, 60, 120, 180, 240, and 300 days). During prevulcanization, the mechanical stability time increased, and the viscosity remained almost constant. The tensile strength increased during storage for a period of 20 days. The degree of crosslinking, modulus, elongation at break, and chloroform number were varied with the time of storage. |
URI: | http://dyuthi.cusat.ac.in/purl/803 |
Files | Size |
---|---|
K K Sasidharan ... fect of the...,Dec2004.PDF | (5.168Mb) |
Abstract: | Prodigiosin is known for its immunomodulatory, antibacterial, antimycotic, antimalarial, algicidal and anticancer activities. Here, we reported the evaluation of prodigiosin pigment as a dyeing agent in rubber latex, paper and polymethyl methacrylate (PMMA) so that it can be considered as an alternative to synthetic pigments. Maximum color shade was obtained in rubber sheet prepared with 0.5 parts per hundred gram of rubber (phr) pigment and PMMA sheet incorporated with 0.08 μg pigment. Results indicate scope for utilization of prodigiosin as dye for PMMA and rubber and also prodigiosin dyed paper as a pH indicator. Further, being a natural and water insoluble pigment, it is ecofriendly |
Description: | African Journal of Biotechnology Vol. 12(17), pp. 2266-2269, 24 April, 2013 |
URI: | http://dyuthi.cusat.ac.in/purl/4263 |
Files | Size |
---|---|
Marine bacteria ... ylate sheets and paper.pdf | (156.6Kb) |
Abstract: | A series of short-isora-fiber-reinforced natural rubber composites were prepared by the incorporation of fibers of different lengths (6, 10, and 14 mm) at 15 phr loading and at different concentrations (10, 20, 30, and 40 phr) with a 10 mm fiber length. Mixes were also prepared with 10 mm long fibers treated with a 5% NaOH solution. The vulcanization parameters, processability, and stress-strain properties of these composites were analyzed. Properties such as tensile strength, tear strength, and tensile modulus were found to be at maximum for composites containing longitudinally oriented fibers 10 mm in length. Mixes containing fiber loadings of 30 phr with bonding agent (resorcinol-formaldehyde [RF] resin) showed mechanical properties superior to all other composites. Scanning electron microscopy (SEM) studies were carried out to investigate the fiber surface morphology, fiber pullout, and fiber-rubber interface. SEM studies showed that the bonding between the fiber and rubber was improved with treated fibers and with the use of bonding agent. |
URI: | http://dyuthi.cusat.ac.in/purl/808 |
Files | Size |
---|---|
Lovely Mathew a ... roperties...,April2006.PDF | (8.573Mb) |
Abstract: | It is observed that reclamation of natural rubber latex based rubber using 2,2'-dibenzamidodiphenvldisulphide as reclaiming agent is an optional methodology for recycling of waste latex rubber (WLR). For progressive replacement of virgin natural rubber by the reclaim, two alternatives curing system were investigated: adjustment or reduction of the curing system with increasing reclaim content, to compensate for the extra amount of curatives brought along by the reclaim. For fixed curing system, as if the reclaim were equivalent to virgin NR. The cure behavior, final crosslink density and distribution, mechanical properties, and dynamic viscoelastic properties of the blends with reclaimed WLR are measured and compared with the virgin compound. The morphology of the blends, sulfur migration, and final distribution are analyzed.The mechanical and dynamic viscoelastic properties deteriorate for both curing systems, but to a lesser extent for fixed curing system compared to adjusted curing system. With the fixed cure system, many properties like tensile strength and compression set do still deteriorate, but tan 6 and Mrrr„/Murxr, representative for the rolling resistance of tires are improved. On the other hand, with the adjusted cure system both mechanical and dynamic properties still deteriorate. |
URI: | http://dyuthi.cusat.ac.in/purl/820 |
Files | Size |
---|---|
V V Rajan and o ... cling of NR...,Feb2006.PDF | (9.335Mb) |
Abstract: | The primary objective of this investigation has been to develop more efficient and low cost adhesives for bonding various elastomer combinations particularly NR to NR, NR/PB to NR/PB, CR to CR,NR to CR and NR to NBR.A significant achievement of the investigation was the development of solventless and environment friendly solid adhesives for NR to NR and NR/PB to NR/PB particularly for precured retreading. Conventionally used adhesives in this area are mostly NR based adhesive strips in the presence of a dough. The study has shown that an ultra accelerator could be added to the dough just before applying it on the tire which can significantly bring down the retreading time resulting in prolonged tire service and lower energy consumption. Further latex reclaim has been used for the preparation of the solid strip which can reduce the cost considerably.Another significant finding was that by making proper selection of the RF resin, the efficiency and shelflife of the RFL adhesive used for nylon and rayon tire cord dipping can be improved. In the conventionally used RFL adhesive, the resin once prepared has to be added to the latex within 30 minutes and the RFL has to be used after 4 hours maturation time maximum shelf life of the RFL dip solution being 72 hours. In this study a formaldehyde deficient resin was used and hence more flexibility was available for mixing with latex and maturing. It also has a much longer shelf life. In the method suggested in this study, formaldehyde donors were added only in the rubber compound to make up the formaldehyde deficiency in the RFL. The results of this investigation show that the pull through load by employing this method and the conventional method are comparable. This study has also shown that the amount of RF resin with RFL adhesive can be partially replaced by other modifying agents for cost reduction.Cashew nut shell liquid (CNSL) resin can be employed for improving the bonding of dipped nylon and rayon cord with NR.Since CNSL resin cannot be added in the dip solution since it is not soluble in water, it was added in the rubber compound. The amount of wood rosin in the rubber compound can be reduced by using CNSL resin.Another interesting result of the investigation was the use of CR based adhesive modified with chlorinated natural rubber for CR to CR bonding. Addition of chlorinated natural rubber was found to improve sea water resistance of CR based adhesive. In the bonding of a polar rubber like nitrile rubber or polychloroprene rubber to a non polar rubber like natural rubber, an adhesive based on polychloroprene rubber was found to be effective. |
Description: | Department of Polymer Science and Rubber Technology, Cochin University of Science and Technology |
URI: | http://dyuthi.cusat.ac.in/purl/2271 |
Files | Size |
---|---|
Dyuthi-T0578.pdf | (6.984Mb) |
Abstract: | The thermal degradation of short kevlar fibre-thermoplastic polyurethane (TPU) composites has been studied by Thermogravimetric Analysis (TGA) and Differential Scanning Calorimetry (DSC). TGA showed that the thermal degradation of TPU takes place in two steps with peak maxima (T1max and T2ma,) at 383°C and 448°C, respectively. In the presence of 10-40 phr of short kevlar fibres, T1_ and T2max were shifted to lower temperatures. The temperature of onset of degradation was increased from 245 to 255°C at 40 parts per hundred rubber (phr) fibre loading. Kinetic studies showed that the degradation of TPU and kevlar-TPU composite follows first-order reaction kinetics. The DSC study showed that there is an improvement in thermal stability of TPU in the presence of 20 phr of short kevlar fibres. |
URI: | http://dyuthi.cusat.ac.in/purl/907 |
Files | Size |
---|---|
Tapan .k Chaki, ... n of short ............PDF | (3.628Mb) |
Abstract: | Scrap latex products contain rubber hydrocarbon of very high quality, that is only slightly crosslinked. A novel economic technique for converting such latex waste into a processible material is developed. This paper reports the effect of adding this latex reclaim to natural rubber. It is shown that latex reclaim can replace raw natural rubber up to about 50 wt.% without affecting mechanical properties. |
URI: | http://dyuthi.cusat.ac.in/purl/843 |
Files | Size |
---|---|
Reena Susan George and Rani Joseph,1993.PDF | (4.752Mb) |
Now showing items 1-11 of 11
Dyuthi Digital Repository Copyright © 2007-2011 Cochin University of Science and Technology. Items in Dyuthi are protected by copyright, with all rights reserved, unless otherwise indicated.