Abstract: | We report enhanced back scattering in nanometer-sized ZnO colloids prepared in two different media, by different methods. The FWHM of the back scattered cone and hence the mean free path varied with concentration of ZnO as well as particle size. The Lorentzian profile of backscattered cone indicates the presence of coherence. |
URI: | http://dyuthi.cusat.ac.in/purl/2587 |
Files | Size |
---|---|
Dyuthi-P0147.pdf | (255.6Kb) |
Abstract: | In the present work, we report the third order nonlinear optical properties of ZnO thin films deposited using self assembly, sol gel process as well as pulsed laser ablation by z scan technique. ZnO thin films clearly exhibit a negative nonlinear index of refraction at 532 nm and the observed nonlinear refraction is attributed to two photon absorption followed by free carrier absorption. Although the absolute nonlinear values for these films are comparable, there is a change in the sign of the absorptive nonlinearity of the films. The films developed by dip coating and pulsed laser ablation exhibit reverse saturable absorption whereas the self assembled film exhibits saturable absorption. These different nonlinear characteristics in the self assembled films can be mainly attributed to the saturation of linear absorption of the ZnO defect states. |
URI: | http://dyuthi.cusat.ac.in/purl/2585 |
Files | Size |
---|---|
Dyuthi-P0145.pdf | (228.9Kb) |
Abstract: | In this paper, the fluorescence behaviour of nano colloids of ZnO has been studied as a function of the excitation wavelength. We have found that excitation at the tail of the absorption band gives rise to an emission that shifts with the change of the excitation wavelength. The excitation wavelength dependent shift of the fluorescence maximum is measured to be between 60 and 100 nm. This kind of excitation wavelength dependent fluorescence behaviour, which may appear to be in violation of Kasha’s rule of excitation wavelength independence of the emission spectrum, has been observed for nano ZnO colloids prepared by two different chemical routes and different capping agents. It is shown that the existence of a distribution of energetically different molecules in the ground state coupled with a low rate of the excited state relaxation processes, namely, solvation and energy transfer, are responsible for the excitation wavelength dependent fluorescence behaviour of the systems. |
URI: | http://dyuthi.cusat.ac.in/purl/1777 |
Files | Size |
---|---|
Excitation wavelength dependent.pdf | (104.7Kb) |
Abstract: | We present the spectral and nonlinear optical properties of ZnO-SiO2 nanocomposites prepared by colloidal chemical synthesis. Obvious enhancement of ultraviolet (UV) emission of the samples is observed, and the strongest UV emission of a typical ZnO-SiO2 nanocomposite is over three times stronger than that of pure ZnO. The nonlinearity of the silica colloid is low, and its nonlinear response can be improved by making composites with ZnO. These nanocomposites show self-defocusing nonlinearity and good nonlinear absorption behavior. The observed nonlinear absorption is explained through two photon absorption followed by weak free carrier absorption and nonlinear scattering. The nonlinear refractive index and the nonlinear absorption increase with increasing ZnO volume fraction and can be attributed to the enhancement of exciton oscillator strength. ZnO-SiO2 is a potential nanocomposite material for the UV light emission and for the development of nonlinear optical devices with a relatively small limiting threshold. |
URI: | http://dyuthi.cusat.ac.in/purl/2608 |
Files | Size |
---|---|
Dyuthi-P0168.pdf | (705.0Kb) |
Abstract: | In this article we present the spectral and nonlinear optical properties of ZnO–TiO2 nanocomposites prepared by colloidal chemical synthesis. Emission peaks of ZnO–TiO2 nanocomposites change from 340 nm to 385 nm almost in proportion to changes in Eg. The nanocomposites show self-defocusing nonlinearity and good nonlinear absorption behaviour. The nonlinear refractive index and the nonlinear absorption increase with increasing TiO2 volume fraction at 532 nm and can be attributed to the enhancement of exciton oscillator strength. ZnO–TiO2 is a potential nanocomposite material for the tunable light emission and for the development of nonlinear optical devices with a relatively small limiting threshold |
URI: | http://dyuthi.cusat.ac.in/purl/1757 |
Files | Size |
---|---|
4.pdf | (316.8Kb) |
Abstract: | In this article we present the nonlinear optical properties of ZnO–TiO2–SiO2 nanocomposites prepared by colloidal chemical synthesis. Nonlinear optical response of these samples is studied using nanosecond laser pulses at an off-resonance wavelength. The nonlinearity of the silica colloid is low and its nonlinear response can be improved by making composites with ZnO and TiO2. These nanocomposites show self-defocusing nonlinearity and good nonlinear absorption behaviour. The nonlinear refractive index and the nonlinear absorption increases with increasing ZnO volume fraction. The observed nonlinear absorption is explained by two photon absorption followed by weak free carrier absorption and nonlinear scattering. ZnO–TiO2–SiO2 is a potential nanocomposite material for the development of nonlinear optical devices with a relatively small limiting threshold. |
URI: | http://dyuthi.cusat.ac.in/purl/2576 |
Files | Size |
---|---|
Dyuthi-P0136.pdf | (245.0Kb) |
Abstract: | In the present work, we have investigated the nonlinear optical properties of self-assembled films formed from ZnO colloidal spheres by z-scan technique. The sign of the nonlinear component of refractive index of the material remains the same; however, a switching from reverse saturable absorption to saturable absorption has been observed as the material changes from colloid to self-assembled film. These different nonlinear characteristics can be mainly attributed to ZnO defect states and electronic effects when the colloidal solution is transformed into self-assembled monolayers. We investigated the intensity, wavelength and size dependence of saturable and reverse saturable absorption of ZnO self-assembled films and colloids. Values of the imaginary part of third-order susceptibility are calculated for particles of size in the range 20–300 nm at different intensity levels ranging from 40 to 325MW/cm2 within the wavelength range of 450–650 nm. |
URI: | http://dyuthi.cusat.ac.in/xmlui/purl/2046 |
Files | Size |
---|---|
Nonlinear optical characteristics of ....pdf | (849.5Kb) |
Abstract: | The laser-induced luminescence studies of the rare earth titanates (R2Ti2O7) (R = La, Nd and Gd) using 355 nm radiation from an Nd:YAG laser are presented. These samples with submicron or nanometer size are prepared by the self-propagating high temperature synthesis (SHS) method and there is no known fluorescence shown by these rare earths in the visible region. Hence, the luminescence transitions shown by the La2Ti2O7 near 610 nm and Gd2Ti2O7 near 767 nm are quite interesting. Though La3+ ions with no 4f electrons have no electronic energy levels that can induce excitation and luminescence processes in the visible region, the presence of the Ti3+ ions leads to luminescence in this region. |
URI: | http://dyuthi.cusat.ac.in/purl/2583 |
Files | Size |
---|---|
Dyuthi-P0143.pdf | (741.3Kb) |
Abstract: | Nanosized ZnO was prepared by polyol synthesis. Fluorescence spectrum of the ZnO colloid at varying pump intensities was studied. The powder was extracted and characterized by XRD and BET. The extracted powder was screen printed on glass substrates using ethyl cellulose as binder and turpinol as solvent. Coherent back scattering studies were performed on the screen printed sample which showed evidence of weak localization. The screen printed pattern showed strong UV emission. |
URI: | http://dyuthi.cusat.ac.in/purl/2511 |
Files | Size |
---|---|
Dyuthi-P0134.pdf | (265.6Kb) |
Abstract: | We have investigated the third-order nonlinearity in ZnO nanocolloids with particle sizes in the range 6-18 nm by the z-scan technique. The third-order optical susceptibility χ(3) increases with increasing particle size (R) within the range of our investigations. In the weak confinement regime, an R2 dependence of χ(3) is obtained for ZnO nanocolloids. The optical limiting response is also studied against particle size. |
URI: | http://dyuthi.cusat.ac.in/purl/2586 |
Files | Size |
---|---|
Dyuthi-P0146.pdf | (755.0Kb) |
Abstract: | In this article we present size dependent spectroscopic observations of nanocolloids of ZnO. ZnO is reported to show two emission bands, an ultraviolet (UV) emission band and another in the green region. Apart from the known band gap 380 nm and impurity 530 nm emissions, we have found some peculiar features in the fluorescence spectra that are consistent with the nanoparticle size distribution. Results show that additional emissions at 420 and 490 nm are developed with particle size. The origin of the visible band emission is discussed. The mechanism of the luminescence suggests that UV luminescence of ZnO colloid is related to the transition from conduction band edge to valence band, and visible luminescence is caused by the transition from deep donor level to valence band due to oxygen vacancies and by the transition from conduction band to deep acceptor level due to impurities and defect states. A correlation analysis between the particle size and spectroscopic observations is also discussed. |
URI: | http://dyuthi.cusat.ac.in/purl/2639 |
Files | Size |
---|---|
Dyuthi-P0326.pdf | (963.7Kb) |
Abstract: | Thermal characterization of alumina–zirconia and zirconia ceramic tapes using a photoacoustic technique is presented. A transmission-mode geometry is employed for the measurement of thermal diffusivity while a reflection-mode geometry is used for the measurement of thermal effusivity. In both these geometries, the same open photoacoustic cell is used. From the measured values of thermal diffusivity and thermal effusivity, the thermal conductivity value has also been evaluated. |
URI: | http://dyuthi.cusat.ac.in/purl/2612 |
Files | Size |
---|---|
Dyuthi-P0172.pdf | (353.2Kb) |
Now showing items 1-12 of 12
Dyuthi Digital Repository Copyright © 2007-2011 Cochin University of Science and Technology. Items in Dyuthi are protected by copyright, with all rights reserved, unless otherwise indicated.