Abstract:
|
ABSTRACT: Polyaniline was synthesized by using ammonium persulfate initiator in the
presence of 1M HC1. It was dried under different drying conditions like room temperature
drying (for 48 h), oven drying (at 50-60°C for 8 h under a vacuum), and vacuum
drying (at room temperature for 16 h). The conductivities of these samples were
measured at microwave frequencies. These samples were also pelletized and the
measurements were repeated. The cavity perturbation technique was used for the
study. |